简介:DD6alloywasbondedbytransientliquidphase(TLP)diffusionbonding.Themaincompositionsoftheinterlayeralloyemployedweresimilartothoseofthebasemetal,DD6,andacertainamountofelementBwasaddedasthemeltingpointdepressant.Theresultsshowthatitisdifficulttoobtainthejointswiththemicrostructurescompletelyhomogeneous.ForthejointTLPdiffusionbondedat1290℃for12h,abouthalfareasofthebeampossessedαγ+γ′microstructure,nearlyidenticalwiththatofthebasemetal,andtheotherlocalareasconsistedofT-solution,borides,etc.Prolongingthebondingtimeto24h,theinhomogeneousareasinthejointreduced,andthejointpropertyimproved.Thejointstress-rupturestrengthat980℃and1100℃reached90%-100%and70%-80%ofthoseofthebasemetalrespectively.