简介:CorrosionbehaviourandbiofoulingcharacteristicsofmildsteelinthreedifferentcoastallocationsintheGulfofMannar,Indiahavebeenstudiedoveraperiodof24months.OysterfoulingwaspredominantatOpensea-Tuticorin,whilebarnaclefoulingwasdominantatbothMandapamandHarbour-Tuticorin.Therateofcorrosionfor24monthsexposureperiodwashighestatMandapam,wherefoulingwasminimal.Thesurfaceofthemildsteelwascharacterizedbyetchings&crevicesbeneaththehardfoulersattachedonit,atallthetestlocations.ThedepthofcrevicecausedbyhardfoulerswashigheratOpensea-TuticorinfollowedbyHarbour-TuticorinandMandapam.ThelossinultimatetensilestrengthwasmoreinOpensea-Tuticorinthantheothertwolocations.Corrosionbehaviourofmildsteelisdiscussedbasedonthevariationinthebiofoulingassemblageatthethreetestlocations.
简介:某地铁钢管柱必须垂直插入柱下扩孔混凝土灌注桩中,柱下C35混凝土初凝时间必须满足钢管柱从插入灌注桩至完成的整个过程,要求混凝土初凝时间不小于36h,终凝时间不大于42h,属于超缓凝混凝土。本文从C35超缓凝混凝土配合比设计思路、原材料的选择与检测、基准配合比设计和对超缓凝混凝土的工作、力学等性能进行检测,得出符合该施工要求的超缓凝混凝土配合比,为以后的类似工程混凝土施工提供可借鉴的经验。