简介:Thecreepmechanismofas-castMg-6Al-6Ndalloywasstudied.Thestressexponentforcreepis5.8undertheappliedstressesof50-70MPaat175°C.Theactivationenergyforcreepis189kJ·mol-1undertheappliedstressof70MPaintherangeof150-200°C.Thetruestressexponentandthresholdstressforcreeparecalculatedas4.96and10.2MPa,respectively.Thetruestressexponentindicatesthatitscreepmechanismbelongstothedislocationclimb-controlledcreep,whichisinagreementwiththemicrostructurechangesbeforeandaftercreep.ThehighvalueforstressexponentisattributedtotheinteractionofAl11Nd3phasewithdislocations.Theactivationenergyismorethantheself-diffusionactivationenergyofMg,whichisattributedtotheloadtransfertakingplacefromthematrixtoAl11Nd3phaseduringcreep.
简介:在H2SO4-Fe2(SO4)3体系中研究载金黄铁矿的浸出动力学,探讨反应温度、Fe3+浓度、硫酸浓度、搅拌速度等对黄铁矿浸出的影响规律。结果表明:在H2SO4-Fe2(SO4)3体系中,在30~75°C下黄铁矿浸出过程主要受化学反应控制Fe3+浓度与黄铁矿的浸出呈正相关,通过Arrhenius经验公式求得浸出表观活化能为51.39kJ/mol。EDS与XPS分析结果表明:黄铁矿氧化过程中硫的氧化经一系列中间形态,最终被氧化成硫酸根,并伴有部分元素硫生成,符合硫代硫酸根氧化路径机理。
简介:采用一种新型高通量实验方法,实现对Ti-5553合金(Ti-5Al-5Mo-5V-3Cr,质量分数,%)在600~700℃范围内的连续温度梯度热处理。实验通过对圆台形样品进行直流电加热,由于截面面积不同而导致电流热效应不同,从而使样品表面温度呈梯度变化。采用端淬实验实现Ti-5553合金的连续冷却速率变化,研究合金在不同热处理条件下的显微组织演变和力学性能。结果表明:Ti-5553合金的伪调幅分解温度为(617±1)℃,析出的α相尺寸在300nm左右;合金在伪调幅分解温度下时效4h达到最高的硬度。因此,这种高通量方法能够快速准确地判断合金中相转变温度以及相应的组织转变。