简介:以便获得对Mg-Ga二进制系统的热力学的描述,对系统的热力学的评价通过Thermo计算用CALPHAD方法被执行?软件包裹基于从出版文学的所有可得到的试验性的数据的评估。答案阶段包括液体,hcp(Mg)并且斜方晶(Ga),被代理答案模型,过量吉布斯精力与Redlich-Kister多项式被表示描述。同时,所有金属间化合的混合物,Mg5Ga2,Mg2Ga,MgGa,MgGa2和Mg2Ga5,作为stoichiometric混合物被建模。在Mg-Ga二进制系统提出各种各样的阶段的吉布斯精力的一套前後一致的热力学的参数最后被获得。好一些的协议在计算结果和报导试验性的数据之间被完成。
简介:Themicrostructuresofas-castandas-solutionMg–12Gd–2Er–1Zn–0.6Zralloyswereinvestigatedbyopticalmicroscopy(OM),scanningelectronmicroscopy(SEM),transmissionelectronmicroscopy(TEM),highresolutiontransmissionelectronmicroscopy(HRTEM)X-raydiffraction(XRD)andselected-areaelectrondiffraction(SAED)inthepresentinvestigation.TheresultsshowthattheprimaryeutecticphaseMg5(Gd,Er,Zn)andsomeflocculentfeaturesarefoundintheas-castalloy;theSAEDpatternindicatesthattheseflocculentfeaturesarethedenseareasofstackingfaults.The14H-LPSOstructureprecipitatesinthetemperaturerangeof673–793K,andthevolumefractionof14H-LPSOstructureincreaseswiththeextensionofheatingtime;however,thereisnoprecipitationof14H-LPSOstructurewhenthetemperaturereachesupto803K.Inaddition,theMg5(Gd,Er,Zn)phasedissolvesgraduallyalongwiththeprecipitationof14H-LPSOstructure.
简介:本文介绍了一种适应于无铅焊料的电子电路基板,是在传统的环氧树脂和酚醛树脂类固化剂组合成的新型树脂中,加入能遏制树脂组成物热膨胀的无机填料而制成的。研发者研究了该基板中添加的无机填料的种类、形状、分类,包括填料的添加量、粒径大小、分散性等,获得了减少由于低树脂流动性及高钻孔加工磨损性所带来的不良影响,确保了这类基板材料的高耐热性和附着性,并且可实现与普通FR-4同等的除钻污性。上述开发产品与传统基板材料制成的电子线路基板相比,热分解温度降低了20℃,铜箔剥离强度提高了0.1kN/m,热膨胀率减少了6×10^-6/℃,即使在温度循环试验中也具有优异的绝缘性和的导通可靠性。且除钻污性时也可用通用的工序进行加工。
简介:散热问题已成为电子设计者面前的最大挑战之一,研究开发导热性好并且与铜箔(铜线路)间有较好的粘结强度和刚度的绝缘层材料对HDI电路板的应用具有重要意义。随着2008年欧盟RoHS指令的逐步开始实施,现有电子元器件含溴阻燃体系逐渐禁用,因此无卤2W导热率导热膜开发意义重大。
简介:Theobjectiveofthisstudyistoinvestigatetheinfluenceofaddingtinyamountofmixedrareearth(La,Ce)andSrtoAl-20Cu-5Si-2Nifillermetal,byanalyzingthemicrostructure,wettabilityandmechanicalpropertiesofbrazedjoints.Theresultsshowthawiththeadditionofmixedrareearth(La,Ce)intoAl-20Cu-5Si-2Nialloy,theα-AlsolidsolutionaswellasCuAl_2(Ni)intermetalliccompoundphasesignificantlyreduced,whilemoreAl-SieutecticphaseandAl-Si-Cuternaryeutecticphasewereproduced.Andasmixedrareearth(La,Ce)addedin,thewettabilityofAl-20Cu-5Si-2Nifillermetaldecreased,whiletheshearstrengthofthebrazedjointsincreased.TheadditionofMinorSrmodificatedAl-20Cu-5Si-2Nifillermetal,furtherreducedtheCuAl_2(Ni)intermetalliccompoundphase,whichwaspartiallyreplacedAl-Si-Cuternaryeutecticphase.Asaresult,thetensilestrengthaswellasthewettabilityofthefillermetalwasimproved.
简介:通过电化学技术分析镁空气电池阳极Mg-Al-Pb-La合金的放电行为,并与Mg-Al-Pb合金的放电行为进行比较.结果表明,相对于Mg-Al-Pb合金,Mg-Al-Pb-La合金在开路电位下耐蚀性增强,表现出更好的放电活性.Mg-Al-Pb-La合金阳极的利用效率比商用Mg-Al-Zn(AZ)和Mg-Al-Mn(AM)合金阳极的利用效率高.由Mg-Al-Pb-La阳极和空气阴极组成的单个镁空气电池的平均放电电压为1.295V,在放电电流密度为10mA/cm2时其放电容量为1370mA·h/g,比Mg-Li合金作为空气电池阳极时的放电容量高.Mg-Al-Pb-La阳极放电性能的增强是由于显微组织的改变降低了自腐蚀,加速了电池放电过程中氧化产物的脱落.另外,分析了Mg-Al-Pb-La合金阳极在放电过程中的溶解机制.