简介:(Y,Gd)BxV1-xO4-x:Eu3+phosphorswerepreparedbysolidstatereaction.Theredemissioncolorpurityof(Y,Gd)BxV1-xO4-x:Eu3+phosphorismuchbetterthanthatoftherecentwidely-usedcommercialredemittingphosphor(Y,Gd)BO3:Eu3+anditsrelativeemissionintensityis84%ofthecommercialphosphor(Y,Gd)BO3:Eu3+.Itisexpectedthat(Y,Gd)BxV1-xO4:Eu3+phosphorwillbeapromisingcandidateforPDP(plasmadisplaypanels)application.
简介:CeO2andCuOx-CeO2supportedpotassiumcatalystsweresynthesizedbywetnessimpregnationmethod.ThecatalystswerecharacterizedbyBET,NO-TPO,NOx-TPDandsoot-TPOmeasurements.Bythedecorationofpotassiumandcopper,themaximumsootcombustiontemperatureoftheceria-basedcatalystdecreasedto338and379°CinthepresenceandabsenceofNOunderaloosecontactmode,re-spectively.ThepronouncedlyenhancedNOoxidationabilitybycopperintroductionandNOxstoragecapacitybypotassiummodif...
简介:
简介:ThemeasurementsoftemperaturedependenceofthemagneticsusceptibilityofLa1-xSrxCoO3perovskiteoxidesatdifferentSrdoping(0≤x≤0.5)andannealingtemperaturewerepresented.Forthesamplewithx=0.1,ashoulderwasobservedaround150K,andapeakwhichisonefeatureofspinglassappearedaround50Kinthecurveofsusceptibilityversustemperature.Thehigh-temperature(250~420K)susceptibilityfitswellwithCurie-Weisslawforallsamples.WeissconstantandeffectivemagneticmomentweredeterminedandtheirvariationswithSrdopingandoxygenannealingconditionwereobtained.TheWeissconstantincreasesmonotonouslywithSrcontentforx>0.2.Thevaluesofeffectivemomentswereinterpretedwiththespinstateofcobaltions.Studiesonthesusceptibilitiesofthesampleswithx=0.2underdifferentpreparationtemperaturesandannealingtemperaturesshowthattherisingofsinteringtemperatureandannealingtemperaturewillincreasethepara-ferromagnetictransitiontemperature,andreducetheeffectivemomenttonormalvalue.OurresultshowsthatbothCo3+andCo4+ionsshouldbeinISstateafterannealingandtheoxygenannealingcausesthetransitionofCo3+spinstatefromHStoIS.
简介:MeltspinningtechnologywasusedtopreparetheMg2Ni-type(Mg24Ni10Cu2)100–xNdx(x=0,5,10,15,20)alloysinordertoobtainananocrystallineandamorphousstructure.TheeffectsofNdcontentandspinningrateonthestructuresandelectrochemicalhydrogenstorageperformancesofthealloyswereinvestigated.ThestructurecharacterizationsofX-raydiffraction(XRD),transmissionelectronmicroscopy(TEM)andscanningelectronmicroscopy(SEM)linkedwithenergydispersivespectroscopy(EDS)revealedthattheas-spunNd-freealloydisplayedanentirenanocrystallinestructure,whereastheas-spunNd-addedalloysheldananocrystallineandamorphousstructureandthedegreeofamorphizationvisiblyincreasedwiththerisingofNdcontentandspinningrate,suggestingthattheadditionofNdfacilitatedtheglassformingoftheMg2Ni-typealloy.TheelectrochemicalmeasurementsindicatedthattheadditionofNdandmeltspinningimprovedtheelectrochemicalhydrogenstorageperformancesofthealloyssignificantly.Thedischargecapacitiesoftheas-castandspunalloysexhibitedmaximumvalueswhenNdcontentwasx=10,whichwere86.4,200.5,266.3,402.5and452.8mAh/gcorrespondingtothespinningrateof0(As-castwasdefinedasthespinningrateof0m/s),10,20,30and40m/s,respectively.Thecyclestability(S20,thecapacitymaintainrateat20thcycle)oftheas-castalloyalwaysrosewiththeincreasingofNdcontent,andthoseoftheas-spunalloysexhibitedthemaximumvaluesforNdcontentx=10,whichwere77.9%,83.4%89.2%and89.7%,correspondingtothespinningrateof10,20,30and40m/s,respectively.
简介:Whitebody-color(Y,Gd)BxV1-xO4-x:Eu3+phosphorswerepreparedbycoprecipitationreaction.UnderVUVexcitationat147nm,theredemissioncolorimetricpurityof(Y,Gd)BxV1-xO4-x:Eu3+phosphorismuchbetterthanthatofcommercialPDP(plasmadisplaypanels)phosphor(Y,Gd)BO3:Eu3+.Butitsrelativeemissionintensityisonlyabout90%ofthecommercialphosphor.
简介:ThemagneticpropertiesandthephasestructureofTb1-xPrxFe1.96(x=0,0.1,...,0.7)werestudied.ItisfoundthatthesaturationmagnetizationoneasyaxisisdecreasedwithincreaseofPrcon-tent,from77.24Am^2·kg^-1forx=0,reducestominimumvalueof11.84Am^2·kg^-1forx=0.5,andreturnesto37.14Am^2·kg^-1forx=0.7.Thenon-cu-bicphasesappearbeyondx=0.2andthematrixchangesfrom1:2phaseforx=0to1:3phaseforx=0.4,atlastto2:17phaseforx=0.7.Thecom-poundsstructurewouldturnmorecomplexasthePrcontentincreases.
简介:AseriesofCe-Fe-Zr-O(x)/MgO(xdenotesthemassfractionofCe-Fe-Zr-O,x=10%,15%,20%,25%,30%)complexoxideoxygencarriersforselectiveoxidationofmethanetosynthesisgaswerepreparedbytheco-precipitationmethod.ThecatalystswerecharacterizedbymeansofX-raydiffractionandH2-TPR.TheXRDmeasurementsshowedthatMgFeO4particleswereformedandFe2O3particleswelldispersedontheoxygencarriers.Thereactionsbetweenmethanedilutedbyargon(10%CH4)andoxygencarrierswereinvestigated.SuitablecontentofCeO2/Fe2O3/ZrO2mixedoxidescouldpromotethereactionbetweenmethaneandoxygencarriers.Therearemainlytwokindsofoxygenofcarriers:surfacelatticeoxygenwhichhadhigheractivitybutlowerselectivity,andbulklatticeoxygenwhichhadloweractivitybuthigherselectivity.Amongallthecatalysts,Ce-Fe-Zr-O(20%)/MgOexhibitedthebestcatalyticperformance.Theconversionofthemethanewasabove56%,andtheselectivityoftheH2andCOwerebothabove93%,theratioofH2/COwasstableandapproachedto2foralongtime.
简介:ThetransportpropertieswerestudiedforrareearthmanganeseoxideLa0.67Cao.33Mn1-xFexO3(x=0-O.3)systems.ItisfoundthatwithincreasingFe^3+-dopingcontentx,theresistanceincreasesandtheinsulator-metaltransitiontemperature(T1M)shiftstolowertemperature.Ifthedopingcontentissmall,thetransportpropertiesmanifestmetalliccharacteristicsinthetemperaturerangeofT<T1M,whiletheywillobeyathermalactivationmodelinthetemperaturerangeofT>T1M.SuchabehaviormaybeattributedtotheFe^3+-dopingandpossibleMnionsscatteringtoelectrons.TheFe^3+dopingmayleadtotheformationofFe^3+-O^2--Mn^4+channels,whichcouldterminatethedoubleexchangeMn^3+-O^2--Mn^4+channels.TheantiferromagneticclustersofFeionsmayinducetheMnionstoscettertotheelectrons.
简介:InordertoimprovethehydrogenationanddehydrogenationperformancesoftheMg2Ni-typealloys,MgwaspartiallysubstitutedbyLainthealloy,andmeltspinningtechnologywasusedforthepreparationoftheMg20-xLaxNi10(x=0,2,4,6)hydrogenstoragealloys.ThestructuresofthealloyswerestudiedbyX-raydiffraction(XRD),scanningelectronmicroscopy(SEM)andhigh-resolutiontransmissionelectronmicroscopy(HRTEM).Itwasfoundthatnoamorphousphaseformedintheas-spunLa-freealloy,buttheas-spunalloyscontainingLaheldamajoramorphousphase.WhenLacontentx≤2,themajorphaseintheas-castalloyswasMg2Niphase,butwithfurtherincreaseofLacontent,themajorphaseoftheas-castalloyschangedintoLaNi5+LaMg3phase.Thermalstabilityoftheas-spunalloyswasstudiedbydifferentialscanningcalorimetry(DSC),showingthatspinningratewasanegligiblefactoronthecrystallizationtemperatureoftheamorphousphase.Thehydrogenabsorptionanddesorptionkineticsoftheas-castandas-spunalloysweremeasuredusinganautomaticallycontrolledSievertsapparatus,confirmingthatthehydrogenabsorptionanddesorptioncapacitiesandkineticsoftheas-castalloysclearlyincreasedwithrisingLacontent.ForLacontentx=2,theas-spunalloydisplayedoptimalhydrogendesorptionkineticsat200°C.