简介:Inordertorealizetheco-firingwithAg/Pdelectrodesinmultilayerdevices,Pb(Zn1/3Nb2/3)1-,-yZrxTiyO3(0.25<x<0.35,0.25<y<0.35)piezoelectricceramics(hereafterdesignatedPZN-PZT)modifiedbyLa2O3hasbeenpreparedbyconventionaltechniquewithsinteringtemperaturefrom1100℃to1140℃.X-raydiffractionpatternsdemonstratedthatpureperovskitephasewasobtained.Secondaryelectronimage(SEI)showedthatcrystallinegrainsinceramicswerewellgrown.d33ofmanufacturedsamplewasashighas560×10-12C/N.kpwasabout0.61andtgδabout30×10-3.TheexistenceofliquidphaseexaminedbyelectrondiffractioninPZN-PZTsampleisbeneficialtosinteringoftheceramic.
简介:Nd_2Zr_2O_7isbeingexploredasanalternatethermalbarriercoating(TBC)materialforoperatingabove1300°C,andgreatefforthasbeenmadetoenlargeitsthermalexpansioncoefficient(TEC)andimproveitstoughness.Inthisstudy,Sc_2O_3wasdopedtoNd_2Zr_2O_7.Thephasestructure,TECsandtoughnessof((Nd_(1-x)Scx))_2Zr_2_O7(x=0,0.025,0.05,0.075,0.1)compoundswereinvestigated.((Nd_(1-x)Scx))_2Zr_2_O7(x=0,0.025,0.05,0.075)exhibitedpyrochlorestructure,while((Nd_(0.9)Sc_(0.1)))_2Zr_2O_7consistedofpyrochloreandfluoritephases.WiththeincreaseoftheSc_2O_3content,theorderingdegreeofthepyrochloreinthecompoundsdecreased.In((Nd_(1-x)Scx))_2Zr_2O_7series,((Nd_(0.925)Sc_(0.075)))_2Zr_2O_7exhibitedthelargestTEC,whilethetoughnessofthecompoundsincreasedwithincreasingtheSc_2O_3content.Therelatedmechanismswerediscussedbasedonthecrystalstructureanalysis.ConsideringtheTECandtoughness,10mol%Sc_2O_3wassuggestedastheoptimaldopingcontentforNd_2Zr_2O_7ceramic.
简介:采用柠檬酸溶胶-凝胶法制备了稀土Gd3+掺杂的LaPU新型热障涂层用陶瓷粉体LaPO4(X=0.0,0.1,0.2,0.3;LGPO)。通过X-ray衍射、扫描电子显微镜、TpDSC、高温热膨胀仪和激光热导仪对样品的相组成、微观形貌、热行为、热膨胀系数和热导率进行表征。结果表明:稀土Gd3+掺杂的LGPO保持了独居石相结构;添加稀土Gd3+不仅可以降低材料的导热系数,还有利于其热膨胀系数的提高;随着稀土Gd3+掺杂量的增加,晶体中点缺陷浓度不断升高,声子平均自由程不断减小,使得稀土Gd3+掺杂的LGPO的热导率在x=0.3时达到最低值(λ=1.22w/(m·K),T=1273K),该值明显低于同温度下8YSZ的热导率。Gd3+掺杂的LaPO4体系是下一代新型热障涂层用陶瓷热门的候选材料之一。
简介:AseriesofCd1-xZnxS/K2La2Ti3O10compositesweresynthesizedviaasimpleco-precipitationmethod.ThepreparedsampleswerecharacterizedbyX-raydiffraction(XRD),scanningelectronmicroscopy(SEM),X-rayenergydispersivespectroscopy(EDX),ultraviolet-visiblediffusereflection(UV-Vis),X-rayphotoelectronspectroscopy(XPS)andphotoluminescence(PL)measurements.ThecompositestructuresconsistedofCd1-xZnxSnanoparticlesevenlydistributedonthesurfaceofK2La2Ti3O10.TheabsorptionedgeofK2La2Ti3O10shiftedtothevisiblelightregionuponintroductionoftheCd1-xZnxSnanoparticles.Thephotocatalyticactivitiesofthecatalystswereevaluatedbyhydrogenproductionundervisiblelightirradiation.ThepreparedCd0.8Zn0.2S(30wt%)/K2La2Ti3O10exhibitedhigherphotocatalyticactivity,evolving6.92mmol/gH2undervisiblelightirradiationfor3h.ThepromotedphotocatalyticactivityofthecompositeswasattributedtothesynergisticeffectbetweenCd1-xZnxSandK2La2Ti3O10,whichresultedinenhancedseparationofphotogeneratedelectronsandholes.