简介:ThehotdeformationbehaviorofTC18alloyatstrainratesrangingfrom1910-4to1910-2s-1andtemperaturesrangingfrom25to800°CwasstudiedusingaWDW-300electronicuniversaltestingmachine.Therelationshipsbetweentruestressandtruestrainshowthatflowstressdecreaseswiththeincreaseoftemperatureandincreasesasstrainrateincreases.Theeffectofstrainrateontheflowstressbecomespronouncedathighertemperatures.Atroomtemperature,theriverpatterncharacteristicofbrittlefractureandthedimplepatterntypicalofductilefracturearefoundtoexistindifferentregionsoffracturesurfacesofthesamples.AnimprovedconstitutiverelationshipisproposedtoaccuratelydescribetheflowstressofTC18byconsideringtheeffectofstrain.Andamicroscopicmodelisalsodeducedwhichcanlinkthephysicalmechanismstothemacroscopicexperimentalresults.Agoodagreementisobtainedbetweenthepredictionsofthemicroscopicmodelandtheresultsofthemacroscopicexperiment.
简介:Nb-24Ti-18Si-2Al-2Hf-4CrandNb-24Ti-18Si-2Al-2Hf-8Cralloyswerepreparedbyarcmeltinginawater-cooledcrucibleunderargonatmosphere.Microstructuralcharacteristicsandoxidationresistanceofthealloysat1250℃wereinvestigated.Theresultsshowthat,whentheCrcontentis4at%,themicrostructuresconsistof(Nb,Ti)_(ss)andNb_5Si_3;asCrcontentincreasesto8at%,C14LavesphaseCr_2Nbisformed.Theisothermaloxidationtestsshowthattheoxidationkineticsofthetwoalloysfollowsimilarfeatures.Theweightgainsofthetwoalloysafteroxidationat1250℃for100hare235.61and198.50mg·cm~(-2),respectively.Duringoxidation,SiO_2,TiO_2,Nb_2O_5andCrNbO_4areformedatfirst.Then,Ti_2Nb_(10)O_(29)isformedafteroxidationfor20minandbeginstochangeintoTiNb_2O_7astheoxidationproceeds.SiO_2isformedassolidstateatfirstbutlaterevolvesintoglassystatetoimprovethecohesionofthescale.Afteroxidationfor100h,oxidationproductsconsistofSiO_2,TiNb_2O_7,Nb_2O_5andCrNbO_4.
简介:1Cr18Ni9Ti不锈钢球头在焊接后经酸洗,表面存在粗糙的腐蚀凹坑。通过采用S-3700N扫描电子显微镜、能谱分析仪、金相显微镜等对表面粗糙的腐蚀凹坑进行成因分析。结果表明:球头在焊接过程中产生了局部敏化现象,球头的晶粒组织细于与之配合的外套螺母组织,使得球头的耐腐蚀性低于外套螺母,在酸洗去氧化皮的过程中,外套螺母与球头的焊缝区、接管嘴的焊缝区之间形成缝隙,酸洗液中的正负离子移动受到了阻滞,导致缝隙处发生严重腐蚀,最终表现为球头表面的点状腐蚀形貌。定期更换酸洗槽液,降低Cl-浓度,以及在酸洗过程中活动零件,可以减少该类腐蚀的产生。
简介:0Cr18Ni9不锈钢薄壁产品在酸洗过程中易发生过腐蚀。本研究采用0.1mm厚度0Cr18Ni9不锈钢带,对酸洗的各影响因素进行试验研究,结果表明:材料状态不同,耐腐蚀能力不同,退火态更易出现过腐蚀;酸液温度、浓度及酸洗的时间均对不锈钢带腐蚀程度和力学性能有较大影响;在含HF的腐蚀剂中酸洗容易使薄壁不锈钢带力学性能降低,造成材料脆化,且HF含量越高对薄壁不锈钢力学性能影响越大。