Crystal Growth and Laser Characteristics of Nd^3+ :KGd(WO4 )2

在线阅读 下载PDF 导出详情
摘要 TheNd3+3.2%(atomfraction):KGd(WO4)2crystalwasgrownbyKyropoulosmethod.TheabsorptionspectrumandfluorescencespectrumofNd3+:KGWcrystalweremeasured.Theabsorptioncrosssectionsat808nm(0.6799×10-20cm2)werecalculated,andtheoutputwavelengthoffluorescenceis1064and1351nm.Thediode-pumpedlaserwasoperatedbothinthefree-runningandpassivelyQ-switchedoperatingmodes.Themaximumlaseroutput(1064nm)is326mWwith62.7%slopeefficiencywheninputenergyis900mW.ThebeamqualityfactorM2≈1.1.Thegreenlightof532nmisobtainedinfrequencydoublingoperation.ThelaserispassivelyQ-switchedbyusingCr4+:LuAGassaturableabsorber.Thepulsewidthis170nsatrepetitivefrequencyof15kHZ.
机构地区 不详
出版日期 2005年06月16日(中国期刊网平台首次上网日期,不代表论文的发表时间)